96% 未致密硅粉
- 二氧化硅: >96%
- 颜色: 深灰色, Grey
- PH Value: 6~8
- 体积密度: 200~350kg/m3, 550~650kg/m3, Above 700kg/m3
- Packages:1000kg plastic woven bags, 10公斤水溶纸袋, 20公斤水溶纸袋, 25kg plastic woven bags, 500kg plastic woven bags, 600kg plastic woven bags, 950kg plastic woven bags
介绍
96% Undensified Silica Fume is a micro-silica fume with 96% 二氧化硅含量, and the Bulk density is 250-400kg/m³.
Silica fume has been used to improve refractory materials for more than 40 年. Silica fume used in refractory materials will have the following characteristics:
1. Improve the flowability of pouring refractory, reduce water consumption, 使其易于成型, 并大大提高生产效率;
2. Due to the intercalation effect of its ultrastructure, the compactness and strength of refractories are greatly improved;
3. Silica fume has high activity, and under the premise of the presence of Al2O3 components, it is easier to generate Mullite phase, which makes the high-temperature strength and thermal shock of refractory material significantly improved.
优点
参数
SLICA FUME | 结果 |
二氧化硅 (%) | 96 |
水分 (%) | 0.46 |
Alkalis like Na₂O (%) | 0.47 |
游离氧化钙 (%) | 0.09 |
Si (%) | 0.12 |
Free CI% (%) | 0.002 |
SO₃ (%) | 0.2 |
L.O.I (%) | 3.7 |
比表面积 (mg) | 22 |
尺寸 | 0.14 |
Accelerated PozzolanicActivity ( 7 天 ) | 126 |
应用
- 水利水电工程: 在防渗、抗磨损部位, 与微硅粉混合后, 可以大大提高防渗, 抗裂, 抗磨损和抗气蚀性能.
- 高强混凝土的生产: 硅粉作为外加剂制备高强混凝土, 实际应用其强度等级可达到100Mpa.
- 海港工程: 掺入硅粉的混凝土可提高混凝土的抗磨性能, 防渗性能, 防止钢筋电化学腐蚀.
- 交通工程: 用于高速公路路面和飞机跑道的硅粉混凝土, 可大大提高混凝土的早期强度和耐磨性, 在公路路面的养护和维修中, 可以提前开放时间,增加经济效益.
- 喷射混凝土: 显着提高塑性混凝土的粘附性能和内聚力, 大幅减少反弹量, 一旦形成,增加喷射混凝土的厚度, 缩短工期,节约工程成本.
包装
- 10kg 水溶纸袋 x 84 在托盘上.
- 20kg 水溶纸袋 x 42 在托盘上.
- 950kg塑料编织袋x 2 在托盘上(带或不带底部喷嘴)
- 1000kg塑料编织袋x 2 在托盘上(带或不带底部喷嘴 )
- 500kg塑料编织袋x 2 在托盘上 (带或不带底部喷嘴 )
本机经筛网自动包装过滤, 以免杂物混入.
Request a Quote
中国领先的微硅粉制造商
HSA拥有先进的生产设备和标准的实验仪器, 并与多家知名跨国公司保持密切联系和战略合作.